1. Micron. 2000 Oct;31(5):571-80.
EELS analysis of cation valence states and oxygen vacancies in magnetic oxides
2. Determination of Oxygen Vacancy Concentration in a Thin Film of La0.6Sr0.4CoO3–delta by an Electrochemical Method。 J. Electrochem. Soc., Volume 149, Issue 7, pp. E252-E259 (July 2002)
3。www.honeywell.com/sites/servlet/com.merx.npoint
,
请大家帮帮忙啊,谢谢大家了!
一般来说,红外,Raman, XRD等都可以测试。缺陷浓度可以影响吸收峰的位置和强度。也可以用其它办法进行测试。可以检索一下文献。如:
1. Micron. 2000 Oct;31(5):571-80.
EELS analysis of cation valence states and oxygen vacancies in magnetic oxides
2. Determination of Oxygen Vacancy Concentration in a Thin Film of La0.6Sr0.4CoO3–delta by an Electrochemical Method。 J. Electrochem. Soc., Volume 149, Issue 7, pp. E252-E259 (July 2002)
3。www.honeywell.com/sites/servlet/com.merx.npoint
,
如果是外延方法得到的单晶,可以用最新的扫描显微术,具体的忘记了,去年的报道,可以测的氧空位的位置
谢谢上面的同学,第2篇和第3篇文献没找到,你能发给我一下吗?谢谢了,我的邮箱xiangsitian@163.com
不是单晶,是烧的粉。
可以用TG 或O2--TPD