[求助] 求英语牛人帮忙翻译一下~~

是一篇专利,有链接~~https://patft.uspto.gov/netacgi/ ... 1&RS=PN/4186121全篇有点长,俺只想知道杜邦公司的聚四氟乙烯膜制备过程中用了哪些物质,(*^__^*) 嘻嘻……不胜感激

» 猜你喜欢

» 本主题相关价值贴推荐,对您同样有帮助:

已阅   关注TA 给TA发消息 送TA红花 TA的回帖
回帖置顶 ( 共有1个 )

154696523

金虫 (著名写手)

正能量使者

【答案】应助回帖

★ ★
haowenjing: 金币+2, 博学EPI+1, 有帮助 2013-02-20 09:10:49
用了如下一些物质:855克固体石蜡、21.8 kg 纯净水、3克全氟辛酸铵(C-8 APFC) ;
0.20 g 过硫酸铵引发剂、25 ml 六氟丙烯还有1360克的四氢呋喃(TFE).
Positive energy makes life better
6楼2013-02-19 20:43:41
已阅   关注TA 给TA发消息 送TA红花 TA的回帖
普通回帖

154696523

金虫 (著名写手)

正能量使者

【答案】应助回帖

这个范围好像有点广,偏离了翻译这一主题了
Positive energy makes life better
2楼2013-02-19 11:02:27
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

haowenjing

银虫 (正式写手)

引用回帖:
2楼: Originally posted by 154696523 at 2013-02-19 11:02:27
这个范围好像有点广,偏离了翻译这一主题了

嘿嘿,好像是有点,要不就前面两段和最后一段,看得行不?
3楼2013-02-19 18:17:23
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

154696523

金虫 (著名写手)

正能量使者

【答案】应助回帖

复制粘贴过来吧,还是不知道您所指?
Positive energy makes life better
4楼2013-02-19 18:23:56
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

haowenjing

银虫 (正式写手)

引用回帖:
4楼: Originally posted by 154696523 at 2013-02-19 18:23:56
复制粘贴过来吧,还是不知道您所指?

貌似想知道的东西在这一段吧A horizontally disposed, water/steam jacketed, cylindrical stainless-steel autoclave located in a barricade and having a capacity of 36,240 cc and a length-to-diameter ratio of about 1.5 to 1, and provided with a 4-bladed cage-type agitator rotated at 46 rpm and running the length of the autoclave, was evacuated and then charged with 855 grams of paraffin wax, 21.8 kg of demineralized water, and 3.0 grams of ammonium perfluorocaprylate (C-8 APFC) dispersing agent. The autoclave was then heated to 88.degree. C., evacuated and purged with tetrafluoroethylene, after which 0.20 g ammonium persulfate initiator (9.2 ppm) (APS) dissolved in water was added. Then 25 ml of hexafluoropropylene (HFP) was pumped in, and the autoclave was pressured over a period of about 2 minutes to 25.6 kg/cm.sup.2 absolute with tetrafluoroethylene (TFE). Stirring rate and temperature were maintained until polymerization started as evidenced by 0.7 kg/cm.sup.2 drop in pressure. The temperature was immediately raised to 90.degree. C. where it was maintained throughout the polymerization. Additional TFE was then added to maintain the reaction pressure at 25.6 kg/cm.sup.2 until a dispersion of approximately 35 percent solids content (total polymer plus aqueous medium basis) was obtained. After about 1360 grams of TFE had been fed following start of the reaction (4.4 percent solids formed), 1000 ml of 2.7 percent by weight aqueous solution of C-8 APFC dispersing agent was injected continuously at 25 ml/minute into the autoclave to stabilize the dispersion. The TFE feed to the autoclave was terminated after 11,804 grams of TFE was fed, and the pressure was allowed to decrease to 12.3 kg/cm.sup.2 before agitation was stopped and the vapor space of the reactor was vented. The polymerization time from start-up to the time feed was turned off was 57 minutes
5楼2013-02-19 18:41:43
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

北极星

捐助贵宾 (小有名气)

郝文静!!
这是一个美好的世界,等待着我们去发现。
7楼2013-02-19 22:41:16
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

haowenjing

银虫 (正式写手)

引用回帖:
7楼: Originally posted by 北极星 at 2013-02-19 22:41:16
郝文静!!

你是Who呀~~
8楼2013-02-20 09:10:31
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

北极星

捐助贵宾 (小有名气)

引用回帖:
8楼: Originally posted by haowenjing at 2013-02-20 09:10:31
你是Who呀~~

难道真的是你!!
这是一个美好的世界,等待着我们去发现。
9楼2013-02-21 10:25:44
已阅   关注TA 给TA发消息 送TA红花 TA的回帖

haowenjing

银虫 (正式写手)

引用回帖:
9楼: Originally posted by 北极星 at 2013-02-21 10:25:44
难道真的是你!!

楞个?报上名来~~
10楼2013-02-21 14:45:23
已阅   关注TA 给TA发消息 送TA红花 TA的回帖
相关版块跳转 我要订阅楼主 haowenjing 的主题更新
信息提示
请填处理意见