24小时热门版块排行榜    

CyRhmU.jpeg
查看: 2205  |  回复: 12
当前只显示满足指定条件的回帖,点击这里查看本话题的所有回帖

bnuphy

新虫 (小有名气)

[交流] 【讨论】DSSC封装中Surlyn 1702 薄膜的使用已有5人参与

文献中常常见到用Surlyn 1702薄膜封装染料敏化太阳能电池:
The cell was completed by sealing the dye coated TiO2 electrode and Pt electrode of a cell together by a thermal plastics spacer (Surlyn 1702, 25 μm, Solaronix) at 120 °C.

The working and counter electrodes were sandwiched using a frame of thermoplastic (Surlyn 1702) and were laminated for about one minute at ~100 °C in vacuum.

The solar cell was fabricated by hot-pressing the sensitized ZnO electrode onto a counter electrode placing a foil (Surlyn 1702, Dupont) in between. The foils center was cut off over an area of about 0.2 cm− 2, which determines the active solar cell area for all investigated samples.

我想问的是,这样的具体过程是什么?【中括号里是我的疑问】
我的猜测是这样的,不知道对不对,请版上的高手们指点一二:
1.裁好Surlyn薄膜        【是裁成下图中的哪一种】
2.将Surlyn薄膜放在一个电极上
3.将另一个电极放在Surlyn薄膜上,形成一个sandwich的的结构
4.在100到120摄氏度之间向sandwich结构施加一定的压力  【怎么施加压力?施加多大的压力合适?需要用什么工具?】
5.然后向其中导入电解液   【电解液怎么导入?如何避免出现小气泡?】


图片在这:不知道为什么发不上来
http://www.douban.com/photos/photo/339446866/

[ Last edited by bnuphy on 2009-11-5 at 19:49 ]
回复此楼
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

csuhwj

银虫 (小有名气)


小木虫: 金币+0.5, 给个红包,谢谢回帖
请问这样用过后,对电极还可以重复使用吗?
10楼2014-01-05 19:04:16
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖
相关版块跳转 我要订阅楼主 bnuphy 的主题更新
普通表情 高级回复(可上传附件)
信息提示
请填处理意见