24小时热门版块排行榜    

查看: 228  |  回复: 0

tankworm

铜虫 (初入文坛)

[求助] 新手想重复这个实验,大侠指点!!!

HTN-LNMO was prepared by stirring stoichiometric amounts of Ni(CH3COO)2 , Mn(CH3COO)2, and Li(CH 3 COO), and adding oxalic acid as a precipitating agent and acetic acid as an additive. The precursor was pretreated in a poly(tetrafluoroethylene) (Tefl on) container at 150–200 ° C for normally 6–12 h. Then the mixture was stirred vigorously until dry.

请问,这些raw material 都应该是水溶液吗?oxalic acid 作为agent该加多少呀?还有,那个Teflon container是用来实现hydrothermal condition的吗?