To determine the orientation of the as-grown O4 single crystal, the wafers cut perpendicularly to the growth direction was tested by XRD2.. There is only one dot in the XRD2 image. Fig. 4 gives the XRD2 pattern integrated from the XRD2 image, and the peak at 42.7° can be indexed to (400) plane. It means that the O4 single crystals grow along the a-axis direction. According to the phase diagram of 2 system, nostoichiometric will result in the appearance of mixture of Zn2TiO4 and ZnO or ZnTiO3. Due to there is no Z1 or Z2 in XRD and Raman, the component of the as-grown crystal is homogeneous. 最好把修改的地方标出来 万分感谢 |
» 猜你喜欢
酰胺脱乙酰基
已经有9人回复
有时候真觉得大城市人没有县城人甚至个体户幸福
已经有3人回复
CSC & MSCA 博洛尼亚大学能源材料课题组博士/博士后招生|MSCA经费充足、排名优
已经有5人回复
有70后还继续奋斗在职场上的吗?
已经有6人回复
博士延得我,科研能力直往上蹿
已经有7人回复
退学或坚持读
已经有27人回复
面上基金申报没有其他的参与者成吗
已经有5人回复
遇见不省心的家人很难过
已经有22人回复
★
sirljz(金币+1):谢谢交流 2010-04-07 08:58
lliang921(金币+15, 翻译EPI+1): 2010-04-09 08:55
sirljz(金币+1):谢谢交流 2010-04-07 08:58
lliang921(金币+15, 翻译EPI+1): 2010-04-09 08:55
|
To determine the CRYSTAL GROWTH orientation of the as-grown O4 single crystal, the wafers WERE cut IN A DIRECTION perpendicular to the CRYSTAL growth direction FOR XRD2 DETECTION. There is only one PEAK in the XRD2 image. Fig. 4 gives the XRD2 SPECTRA EXTRACTED from the XRD2 image. The peak at 42.7° REPRESENTS (400) plane.THE RESULT INDICATES that the O4 single crystals growED along the a-axis. According to the phase diagram of 2 system, nostoichiometric REACTION USUALLY result in A mixture of Zn2TiO4 and ZnO or ZnTiO3. IN ADDITION, no Z1 or Z2 WERE DETERMINED BY XRD and Raman. THEREFORE, IT IS SAFE TO CONCLUDE THAT the as-grown crystalS HAD A homogeneous STRUCTURE. P.S. 删除的部分没有标记出来。 |
2楼2010-04-07 05:45:20
fatemyself
铜虫 (小有名气)
- 翻译EPI: 6
- 应助: 1 (幼儿园)
- 金币: 82.3
- 帖子: 119
- 在线: 3.3小时
- 虫号: 594288
- 注册: 2008-09-06
- 专业: 电化学
| As to determine the orientation of the as-grown O4 single crystal, the wafers cut perpendicularly to the growth direction was tested by XRD2.. There is only one dot in the XRD2 image. Fig. 4 gives the XRD2 pattern integrated from the XRD2 image, and the peak at 42.7° can be indexed to (400) plane. It means that the O4 single crystals grow along the a-axis direction. According to the phase diagram of 2 system, nostoichiometric will result in the appearance of mixture of Zn2TiO4 and ZnO or ZnTiO3. Due to there is no Z1 or Z2 in XRD and Raman, the component of the as-grown crystal is homogeneous. |

3楼2010-04-07 15:20:09
gjy9814100
金虫 (正式写手)
- 翻译EPI: 5
- 应助: 0 (幼儿园)
- 金币: 1233.6
- 散金: 801
- 帖子: 977
- 在线: 145.6小时
- 虫号: 986262
- 注册: 2010-03-31
- 性别: GG
|
To determine the orientation of ZO single crystal growth, the wafers located at the middle and top of the crystal rod were cut in a direction perpendicular to the crystal growth direction for XRD examination. Results were same at middle and top of the rod. There was only one dot in the XRD image. Fig. 4 illustrated the XRD2 pattern extracted from the XRD2 image. The peak at 42.7° was the reflection of (400) plane. The result indicated that the ZO single crystals growed uniformly along the a-axis. P.S. 删除的部分没有标记出来。 转载:http://muchong.com/bbs/viewthread.php?tid=1932281&fpage=1 |