[求助]
时间分辨 Pl 中weight fraction 什么意思 是怎么算出来 的
|
|
文献中经常遇到time-resolved PL dacay 中有 不同decay lifetime的 weight fraction,请问具体是代表什么 怎么算出来的: Time resolved photoluminescence (PL) behavior was charac- terized to probe the infl uence of the enhanced crystallization of perovskite thin fi lms on charge dissociation. Detailed infor- mation regarding the preparation, measurement, and fi tting methodology can be found in the experimental section. The PL lifetime of the samples was fi tted with a bi-exponential decay function containing a fast decay and a slow decay process. We consider the fast decay process to be the result of the quenching of free carriers in the perovskite domain through transport to PEDOT SS or PC 61 BM, and the slow decay process to be the result of radiative decay. Figure 5 displays the PL decay and the related parameters are summarized in Table 2 . For the pris- tine thin-fi lm perovskite, the fast decay lifetime is 12.9 ± 0.8 ns and the slow decay lifetime is 104 ± 3 ns while their weight fractions are 81% and 19% respectively, |
» 猜你喜欢
广东地区寻找 高温氢气烧结炉
已经有4人回复
广东地区寻找 高温氢气烧结炉
已经有1人回复
金属材料论文润色/翻译怎么收费?
已经有269人回复
广东地区 寻找 高温氢气烧结炉
已经有1人回复
分享外企Sabic与科思创关于PC改性研究方向的报告
已经有0人回复
求助:成都理工大学 《物理学与现代科技》课件
已经有0人回复
酚醛基硬碳的预固化相关问题求助
已经有0人回复
倒贴50元!免费听新材料顶级培训,只需帮我签个到
已经有1人回复
钠电正极材料改性探索丨工艺装备化深度实践
已经有0人回复
Nano-Micro Letters的Awaiting Production Checklist状态
已经有0人回复










SS or PC 61 BM, and the slow decay process to be the
回复此楼