24小时热门版块排行榜    

查看: 872  |  回复: 7

goingabroad

木虫 (文坛精英)

[求助] G-X6CrNi1810

求助G-X6CrNi1810材料的资料或标准。
回复此楼

» 猜你喜欢

» 本主题相关商家推荐: (我也要在这里推广)

» 本主题相关价值贴推荐,对您同样有帮助:

已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

hwweven

至尊木虫 (知名作家)

医疗器械注册和审核

优秀版主

【答案】应助回帖

感谢参与,应助指数 +1
lz看看是不是这个?

Steel PK11SP (Mat.No. 1.4541, DIN X6CrNiTi18-10, AISI 321)
Designation by Standards

Brand Name        Ravne No.        Mat. No.        DIN        EN        AISI
PK11SP        914        1.4541        X6CrNiTi18-10        X6CrNiTi1810        321

Chemical Composition (in weight %)

C        Si        Mn        Cr        Mo        Ni        V        W        Others
max. 0.08        max. 1.00        max. 2.00        18.00        -        10.50        -        -        min. Ti=5 x C x 0.7

Description
The key feature of 321 stainless is its resistance to intergranular corrosion. It employs titanium as a stabilizing element against chromium carbide formation. This alloy also exhibits strength characteristics superior to those of 304 stainless.

Applications
Jet engine parts, furnace heat treated parts, expansion joints, turbo superchargers, oil refiners, exhaust manifolds and high temperature chemical production equipment.

Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 203, 186 (200oC), 172(400oC)
Density [g/cm3]: 7.9
Thermal conductivity [W/m.K]: 14.6
Electric resistivity [Ohm mm2/m]: 0.73
Specific heat capacity[J/g.K]: 0.502

Coefficient of Linear Thermal Expansion 10-6 oC-1

20-100oC        20-200oC        20-300oC        20-400oC        20-500oC
16.0        17.0        17.0        18.0        18.0

Hardening
Harden from a temperature of 1020-1100oC followed by water or air quenching. Structure is austenite with small ferrite component.

Mechanical properties in solution-annealed condition and reistance to intercrystalline corrosion
Hardness: 130-190 HB
0.2 % proof stress: 190 N/mm2
1.0 % proof stress: 225 N/mm2
Tensile strength: 500-700 N/mm2
Elongation: 40% (for d<=160, longit.)
Resistance to interystalline corrosion: yes (in as delivered condition), yes (in sensitised condition)
Note: Sensitisation treatment for 15 min at 700oC with subsequent cooling in air.

Mechanical Properties At Elevated Temperatures

Quenched Condition

Temperature        50oC        100oC        150oC        200oC        250oC        300oC        350oC        400oC
0.2 % proof stress in N/mm2        190        176        167        157        147        136        130        124

Forging
Hot forming temperature: 1150-850oC.

Machinability
Excellent speeds and feeds are capable with this material. The addition of sulfur causes a very brittle chip. Many companies now offer premium machinability grades, such as CarTech with their Project 70 and 7000 series.

Corrosion Resistance
Resistant to a variety of organic and inorganic chemicals, fresh water and atmospheric corrosion.

Welding
Although not recommended, welding may be performed if low temperatures are employed. Recommended filler metal is AWS E/ER312. At high temperature, the sulfur in 303 tends to precipitate at the weld boundary resulting in weak and brittle joints.

Cold working
Minor deformation is possible with this alloy, although it is not its strong point. Type 303 Se is superior in this aspect.

Forms manufactured: Please see the Dimensional Sales Program.       

Disclaimer
The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Unless otherwise specified, registered trademarks are property of Metal Ravne company. Copyright 2011 by Metal Ravne. All rights reserved. Contact our Sales Office for more information.
来源:http://126.am/UZfIe1
2楼2012-08-15 23:10:13
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

goingabroad

木虫 (文坛精英)

引用回帖:
2楼: Originally posted by hwweven at 2012-08-15 23:10:13
lz看看是不是这个?

Steel PK11SP (Mat.No. 1.4541, DIN X6CrNiTi18-10, AISI 321)
Designation by Standards

Brand Name        Ravne No.        Mat. No.        DIN        EN        AISI
PK11SP        914        1.4541        X6CrNiTi18-10        X6CrNiTi1810        3 ...

不是
3楼2012-08-16 07:00:41
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

hwweven

至尊木虫 (知名作家)

医疗器械注册和审核

优秀版主

【答案】应助回帖

引用回帖:
3楼: Originally posted by goingabroad at 2012-08-16 07:00:41
不是...

这个钢材的编号不就是 X6CrNiTi18-10吗?
4楼2012-08-16 07:58:59
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

rwjghost

至尊木虫 (职业作家)

双草籽儿

引用回帖:
4楼: Originally posted by hwweven at 2012-08-16 07:58:59
这个钢材的编号不就是 X6CrNiTi18-10吗?...

这种惜字如金的求助最难搞定。。。。
新虫(10)、铁虫(50)、铜虫(200)、银虫(500)、金虫(1.5k)、木虫(5k)、铁杆木虫(1w)、至尊木虫(5w)、木虫之王(10w)、神虫浮云(9999999)
5楼2012-08-16 08:22:45
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

hwweven

至尊木虫 (知名作家)

医疗器械注册和审核

优秀版主

引用回帖:
5楼: Originally posted by rwjghost at 2012-08-16 08:22:45
这种惜字如金的求助最难搞定。。。。...

是啊,都不知道是想得到哪方面讯息。
6楼2012-08-16 08:36:23
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

rwjghost

至尊木虫 (职业作家)

双草籽儿

引用回帖:
6楼: Originally posted by hwweven at 2012-08-16 08:36:23
是啊,都不知道是想得到哪方面讯息。...

呵呵,等他自己补充信息吧,不然很难解决的;)~
新虫(10)、铁虫(50)、铜虫(200)、银虫(500)、金虫(1.5k)、木虫(5k)、铁杆木虫(1w)、至尊木虫(5w)、木虫之王(10w)、神虫浮云(9999999)
7楼2012-08-16 08:52:03
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

hwweven

至尊木虫 (知名作家)

引用回帖:
7楼: Originally posted by rwjghost at 2012-08-16 08:52:03
呵呵,等他自己补充信息吧,不然很难解决的;)~...

8楼2012-08-16 08:58:14
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖
相关版块跳转 我要订阅楼主 goingabroad 的主题更新
信息提示
请填处理意见