Following calcination, carburization and passivation, the Mg-Mo2C/HY and K-Mo2C/HY catalysts had significantly reduced surface area, total pore volume,micropore area andmicropore volume (Table 1)comparedtothe Mo2C/HY catalyst. However, the surface area was not strongly dependent upon the amount of Mg added, with all the Mg-Mo2C/HY catalysts having surface areas in the range 389–462 m2/g, compared to 522 m2/g for the Mo2C/HY. The relative loss in BET and micropore area with Mg or K addition to the Mo2C/HY, was almost the same. Fig. 1 shows themicropore size distribution of the 2%Mg-Mo2C/HY catalyst compared to the HY zeolite. [ Last edited by ankang276 on 2011-8-9 at 13:18 ] |
» 猜你喜欢
AI论文写作工具:是科研加速器还是学术作弊器?
已经有5人回复
Bioresource Technology期刊,第一次返修的时候被退回好几次了
已经有8人回复
寻求一种能扛住强氧化性腐蚀性的容器密封件
已经有7人回复
到新单位后,换了新的研究方向,没有团队,持续积累2区以上论文,能申请到面上吗
已经有8人回复
申请2026年博士
已经有6人回复
请问哪里可以有青B申请的本子可以借鉴一下。
已经有5人回复
天津工业大学郑柳春团队欢迎化学化工、高分子化学或有机合成方向的博士生和硕士生加入
已经有5人回复
2025冷门绝学什么时候出结果
已经有7人回复
aixun3000
金虫 (小有名气)
- 翻译EPI: 3
- 应助: 0 (幼儿园)
- 金币: 1182.4
- 散金: 50
- 帖子: 78
- 在线: 68.7小时
- 虫号: 1106821
- 注册: 2010-09-24
- 专业: 中药药效物质
3楼2011-08-09 20:41:01
slz146
木虫 (正式写手)
- 翻译EPI: 75
- 应助: 0 (幼儿园)
- 贵宾: 0.055
- 金币: 1657.8
- 散金: 966
- 红花: 7
- 帖子: 713
- 在线: 225.5小时
- 虫号: 1097156
- 注册: 2010-09-13
【答案】应助回帖
★ ★
sltmac(金币+2): 辛苦~ 2011-08-09 14:04:28
ankang276(金币+33, 翻译EPI+1): 2011-08-09 20:48:24
sltmac(金币+2): 辛苦~ 2011-08-09 14:04:28
ankang276(金币+33, 翻译EPI+1): 2011-08-09 20:48:24
| 经过煅烧、碳化以及钝化作用之后,Mg-Mo2C/HY和 K-Mo2C/HY催化剂与Mo2C/HY 催化剂相比,比表面积、总孔容、微孔比表面积以及微孔孔容都显著减少(表1)。但是,由于与Mo2C/HY催化剂522 m2/g 的比表面积相比,所有Mg-Mo2C/HY 型催化剂的比表面积都在389–462 m2/g,所以比表面积并不完全取决于所添加Mg的量。将Mg和K添加到Mo2C/HY催化剂中,二者在BET中测得数据的相对损失及微孔比表面积几乎相同。图1表示的是2%Mg-Mo2C/HY催化剂及HY分子筛的微孔孔径分布。 |