[求助] 无机材料化学专业:麻烦专业人士把一句英语翻译成中文,谢谢!

In general, slow crystallization is
required to form products with a thermodynamically stable structure
because the crystallizing partners have time to recognize each other and
follow the lowest-energy path. However, at 180 °C, the temperature is
high and fast crystallization takes place. This fast crystallization often leads
to kinetically controlled products, such as unstable or metastable crystal
structures, and even defects can be formed during fast nucleation
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

jwdxbjzh

至尊木虫 (职业作家)


Mally89(金币+1): ... 2011-06-17 20:53:41
楼上正解!“相互认别”改为“相互识别”更好!
jwd
3楼2011-06-13 23:15:48
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖
查看全部 3 个回答

爱与雨下

荣誉版主 (职业作家)

木虫讲师

优秀版主

【答案】应助回帖

★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★
sltmac(金币+1): 谢谢交流~~ 2011-06-13 22:28:11
wuyao118(金币+20, 翻译EPI+1): 2011-06-14 16:04:06
sltmac(金币+30): 欢迎常来~~ 2011-06-22 22:10:24
wuyao118(金币+30): 好 2011-07-06 08:34:01
一般情况下,形成一个热力学稳定结构的晶体需要缓慢结晶,这是由于结晶时晶体之间需要时间相互认别, 并且遵循最低能量路径。然而,在180 C时的温度 高,快速结晶就容易发生。这种快速的结晶往往导致 产生动力学控制产品,例如不稳定或亚稳态晶体结构, 甚至在快速成核时可以形成缺陷