[求助] Gd2O3磁性的问题

用VASP算Gd2O3晶体,设置了MAGMOM的值为8 -8 -8 8 8 8 -8 -8 8 -8 8 -8 8 -8 -8 8 8 -8 -8 -8 8 -8 8 8 -8 8 8 -8 8 -8 8 -8 48*0,32个Gd,48个O,反铁磁,为什么优化后,(100)面OUTCAR中Gd的mag=0,完全算不到7这么大的值呢?请教各位,谢谢!
我的INCAR设置为
GGA = 91   
VOSKOWN = 1
POTIM =0.05
LMAXMIX=6  
LDAU=.TRUE.
LDAUTYPE=2
LDAUL=3 -1
LDAUU=7.5 0
LDAUJ=0.6 0
LDAUPRINT=0
NPAR=4         
LPLANE = .TRUE.
LREAL  = Auto               
ENCUT  = 510               
PREC   = Normal              
EDIFF  = 1e-5  
ALGO  = Fast          
NELM=  75      
NELMIN = 6     
#   NELMDL= -5
   ISIF   = 0
MAGMOM =8 -8 -8 8 8 8 -8 -8 8 -8 8 -8 8 -8 -8 8 8 -8 -8 -8 8 -8 8 8 -8 8 8 -8 8 -8 8 -8 48*0
   ISPIN  = 2
#   NUPDOWN=1
   EDIFFG =-2e-2
   NSW    = 300
   IBRION = 2   
#   IOPT =2     
   ISMEAR = 0  
   SIGMA  = 0.1
  LORBIT =11   
LWAVE  = .FALSE.
LCHARG= .FALSE.