Table 1. Formulation of the experimental specimen Table 2. Chemical composition of raw materials
In order to identify the formation temperature of spinel and CA6 according to the thermal change, the mineral facies analysis was carried out by using the XRD(X-ray diffraction) at 1100℃, 1200℃, 1300℃ and 1400℃ using X’pert PRO(PANalytical, Netherland). And the corrosion resistance was measured by using a rotative corrosion
tester, and the ladle slag was used of which the value of CaO/SiO2 was 5.8(CaO/SiO2 = 5.8).
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

cmds1907

铁杆木虫 (著名写手)

【答案】应助回帖

★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★ ★
真强必胜: 金币+1, 谢谢 2014-09-22 18:25:52
wanghao69: 金币+15, 翻译EPI+1, ★★★★★最佳答案, 非常非常感谢 2014-09-22 20:32:11
表1. 实验样品的配方。表2原材料的化学成分以便根据热变化识别尖晶石和CA6的形成温度,矿物相分析由XRD(X射线衍射)在1100℃、1200℃、1300℃和1400℃使用X 'pert PRO(PANalytical、荷兰)进行。耐蚀性用一个回转的腐蚀测试仪测量,且所用钢包渣的CaO/SiO2值是5.8(CaO/SiO2= 5.8)。