24小时热门版块排行榜    

查看: 315  |  回复: 16
当前主题已经存档。
当前只显示满足指定条件的回帖,点击这里查看本话题的所有回帖

zilong272

银虫 (小有名气)

[交流] 镀膜设备讨论

做薄膜的虫虫们说说你们用的是那个单位的镀膜设备啊,可以设置的参数有那些,提拉时有振动吗,镀膜效果怎么样啊。谢谢拉。
回复此楼
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

ElectroWang

铜虫 (小有名气)

gh different engineers count things differently, there are four distinct stages to the spin coating process.

Deposition of the coating fluid onto the wafer or substrate
This can be done by using a nozzle and pouring the coating solution or by spraying it onto the surface. A substantial excess of coating solution is usually applied compared to the amount that is required.

The substrate is accelerated up to its final, desired, rotation speed
The substrate is spinning at a constant rate and fluid viscous forces dominate the fluid thinning behavior
The substrate is spinning at a constant rate and solvent evaporation dominates the coating thinning behavior
11楼2008-04-15 12:19:49
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖
查看全部 17 个回答

suzy866


nxl5096224(金币+1,VIP+0):谢谢参与讨论~
我们实验室用的是自己组装的数控提拉机,可以控制的参数有提拉速度,浸渍时间。我们一般对提拉速度与浸渍时间作为参数进行实验以得出最佳实验效果。本人觉得俺们自己组装的设备还是不错的,性能好且便宜,市场上的太贵了,买不起啊。
2楼2008-01-02 10:19:00
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

zilong272

银虫 (小有名气)

你们的镀膜设备振动大吗,是用什么驱动的啊,我们实验室现在正需要一台这样的设备啊。可以帮我们做一套吗?
3楼2008-01-02 10:48:30
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖

suzy866

★ ★
eric2004(金币+2,VIP+0):多谢您热心应助!
我们采用步进电机驱动无牙丝杆驱动滑块滑动,振动极小。可以做,而且我们现在也想在高校实验室里推广,这样就会使更多实验室可以按自己的实验设计完成实验,而不至于因市场上设备贵而改实验方案。你要是需要的话,可以QQ联系:71479442
4楼2008-01-04 16:31:50
已阅   回复此楼   关注TA 给TA发消息 送TA红花 TA的回帖
普通表情 高级回复 (可上传附件)
信息提示
请填处理意见