As is shown in the Figure 4, when the thickness ratio of the coating and substrate is greater than 1%, there is a inflection point at 150 ° C, when the thickness ratio of the coating and substrate is less than 1%, there is no inflection point at 150 ° C, reflecting that only when the coating thickness reaches a certain thickness (more than 1%),a turning point can be observed from the curve of damping performance at about 150 ° C .