★ 小木虫(金币+0.5):给个红包,谢谢回帖交流
我最近看 锂电的文章 有的用 PVDF 做binder
Electrode slurries, ranging from 86 to 96% active material, were
prepared using appropriate ratios of LiNi1/3Mn1/3Co1/3O2 grade
BC-618K from 3M Co., St. Paul, MN, specific surface area
= 0.26 m2/g, polyvinylidene fluoride PVDF Kynar 301F from
Arkema, Philadelphia, PA, and carbon black Super-S from MMM
Carbon, Tertre, Belgium in an n-methyl pyrrolidone solvent NMP.
They were mixed in a Kurabo Mazerustar Osaka, Japan KK-50S
planetary mixer-deaerator before being spread onto a 0.021 mm
thick current collecting aluminum foil.
摘自 Dahn 的
A Guide to Li-Ion Coin-Cell Electrode Making for Academic Researchers |
|