which was then sealed with a silicon rubber septum and degassed using
several N2/vacuum cycles. The flask was placed in a water bath at 70
°C for 30 min with stirring at 400 rpm. Emulsion polymerization was
begun on addition of a solution of an initiator (KPS: 22 mg or VA-
080: 70 mg) in water (1.0 g).