NanoEnergy® performs better at elevated temperature due to lower internal resistance. When operated at 100 oC, NanoEnergy® can be charged and discharged at higher rate and with higher capacity. Figure 7 shows typical discharge curves of a 0.1 mAh NanoEnergy® discharged at room temperature, 60 oC, and 100 oC. NanoEnergy® can even be operated at temperatures as high as 170 oC, however, the capacity drops much faster during cycling.
![请问关于薄膜锂电的这两个图怎么看呢?谁能解释一下?]()
2017-05-09_155525.jpg
![请问关于薄膜锂电的这两个图怎么看呢?谁能解释一下?-1]()
2017-05-09_155541.jpg |
|