Li2CO3, FeC2O4·2H2O, Mn(COOCH3)2·4H2O and NH4H2PO4 (all
chemicals of 99% purity from Aldrich) and citric acid (Shinyo Pure
Chemicals, 99% purity) were used as the starting materials to synthesize
LMFP composites. These were dissolved in deionized water
at room temperature and to the resulting solution was added citric
acid solution. After homogenous mixing, the sol was dried by
keeping it at 75 ◦C for 12 h during magnetic stirring,
Li2CO3, FeC2O4·2H2O, Mn(COOCH3)2·4H2O and NH4H2PO4 (all
chemicals of 99% purity from Aldrich) and citric acid (Shinyo Pure
Chemicals, 99% purity) were used as the starting materials to synthesize
LMFP composites. These were dissolved in deionized water
at room temperature and to the resulting solution was added citric
acid solution. After homogenous mixing, the sol was dried by
keeping it at 75 ◦C for 12 h during magnetic stirring,
sol-gel 可以用硝酸铁 醋酸铁 不见得非得用草酸亚铁啊
这个我知道,只是打算用草酸亚铁,不想一下就换原料,想先找找解决的办法。
同求!
我也用草酸亚铁的,一直溶解不了,直接用的,呵呵,也没什么大问题。不过能溶解更好了
你们在哪买的草酸亚铁阿,我怎么一直买不到呢。。。。。